The
sampling happens with a carbidetipped driller with a diameter
of 1,4 to 2 mm at low speed. Usually two samples are taken where the
quantity of sample is very small (200mg). |
 |
| |

In
case a restoration is found out during the analysis, it will be mentioned
in the "TL" certificate. Strict confidence of the laboratory
is guaranteed when working out the "TL" certificate. All certificates
are written without mentioning the name of the supplier. |
| |

In
a detailed conversation we determine the procedure and the taking
of samples (quantity and position).
Do
you wish to attend to the analysis? No problem. Also in case of questions
regarding transport for taking samples in the laboratory, at your
place or your visit at our place we will be of assistance for you.
With
regard to the position of problem follows a detailed expert opinion
We
are one of the leading laboratories in this branch since 1979. |
 |
 |
Labor
Ralf Kotalla, Kätzling 2, D-72401 Haigerloch Weildorf
Tel.: 00497474/95360, Fax: 00497474/953610,
Mobile: 0049(0)171/6228521 |
|